Horizontal Flashing & Finning

Cause Remedy
Incorrect powder / water ratio (too much water). Using correct amount of water (especially important with vacuum investing machines).
Work time of investment not used up. Ensuring the work time is used up and slurry temperature is 20 - 22ºC. 
Casting the material at too great a pressure (centrifugal casting). Use the correct spin speed to suit the weight and metal and type of work.
 
        